AATCC 8 Crocking: Dry and Wet Rubbing Specs for Dark Suit Cloth

Ask for dry and wet results on the same lot. AATCC 8 is colorfastness to crocking: a colored textile is rubbed with a white crock cloth under controlled conditions, using dry and wet crock cloths. Results are graded with the Gray Scale for Staining or the Chromatic Transference Scale. The method summary notes it is not recommended for carpets or for prints that are too small for a proper test, and that it may be run before or after washing, drycleaning or other exposures when those conditions matter to the program.

Why do dark suit cloths need both dry and wet crocking?

Navy, charcoal and black suit cloths are the ones buyers most often find on shirts and car seats after early wear. AATCC 8’s design is explicitly two conditions — dry crocking and wet crocking — so a brief that only quotes one number is incomplete. Grade the transfer on the white crock cloth with the Gray Scale for Staining or the Chromatic Transference Scale, and write which scale you used.

Brief itemWhat AATCC 8 summary supportsWhat to write
ConditionsDry and wet crockingBoth results on the same lot
ActionRub colored textile with white crock cloth under controlled conditionsName AATCC 8, not “rub test”
GradingGray Scale for Staining or Chromatic Transference ScaleName the scale on the report
SequenceMay be run before/after washing, drycleaning, etc.State as-received or after which exposure
Out of scope examplesNot recommended for carpets or very small printsSuit cloth is in scope; tiny prints are not

What belongs in the mill / QC brief?

  • Method: AATCC 8, dry and wet
  • Grading scale named (Gray Scale for Staining or Chromatic Transference Scale)
  • Whether the test is on as-received cloth or after a named wash/dryclean exposure
  • Lot / piece number on the report
  • Target grade per condition (buyer’s acceptance number — do not invent one here)

This site does not invent machine stroke counts or moisture pickup percentages that were not confirmed on the opened method page.

How does crocking fit the sample timeline?

Crocking is a cloth property. Collect the AATCC 8 report from the mill before the 7–14 day sample is sealed. Bulk OEM from 50 should cut from a lot that matches that report. Patterns are not resold; NDA available on request if your crocking limits are proprietary.

"Bulk OEM from 50 follows a 7–14 day sample and written approval. Ask for AATCC 8 dry and wet grades on the cloth lot before that sample is sealed." — Shi Yuan Suit Factory (statement built from published factory policy)

FAQ

What does AATCC 8 test on suit cloth?

Colorfastness to crocking: rubbing a colored textile with a white crock cloth under controlled conditions in dry and wet states, then grading the transfer.

How are AATCC 8 results graded?

With the Gray Scale for Staining or the Chromatic Transference Scale.

When should AATCC 8 results reach Shi Yuan?

With the cloth indent, before the 7–14 day sample, so bulk OEM from 50 cuts from a matching lot.

Core factory facts

Contact

WhatsApp +65 8013 8838 · Email houzhenying226@gmail.com

Shi Yuan Suit Factory (Tianjin Shiyuan Tongchuang Technology Co., Ltd.) · Est. 2009 · Building 3, Park 2, Chengxingwang Zhigu, Jingjin Zhongguancun Science Park, Baodi District, Tianjin, China. Acumenwear.com is our English export site.

Previous
Previous

Wool Moisture Regain: Why Suit Cloth Weight Can Feel Different from the Ticket

Next
Next

ISO 3758 Care Labelling Symbols: How Many Symbol Families a Private-Label Suit Needs